Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

ASME Section VIII Div 2-Design by Fatigue Analysis-Interpolation between ultimate tensile strength

Status
Not open for further replies.

prumax

Structural
Joined
Jul 25, 2017
Messages
2
Location
AT
Hi,

I am looking for a way how to consider an intermediate ultimate strenght US (552MPa < US < 793MPa) for an fatigue evaluation acc. ASME Section VIII Div 2.

In the 1989 Addition i found at page 564 "Where curves for various strength levels of a material are given, linear interpolation may be used for intermediate strength levels of these materials".

Unfortunately I can not find anything similar in the latest Versions (2007 - 2015)

Has someone experience with this issue?

Thank you in advance

Markus

 
Specifically, what is your material/strengths?
 
It is XCrNi18-7 / yield = 330MPa / tensile = 630 MPa
 
The last sentence of 3-F.1.2(a) covers you. However, I would have thought that your material would fall under sub-paragraph (b).

Use the 2017 Edition curves - they're easier to code. And pay attention to the maximum temperature limits, too.
 