Hi,
I am looking for a way how to consider an intermediate ultimate strenght US (552MPa < US < 793MPa) for an fatigue evaluation acc. ASME Section VIII Div 2.
In the 1989 Addition i found at page 564 "Where curves for various strength levels of a material are given, linear interpolation may be used for intermediate strength levels of these materials".
Unfortunately I can not find anything similar in the latest Versions (2007 - 2015)
Has someone experience with this issue?
Thank you in advance
Markus
I am looking for a way how to consider an intermediate ultimate strenght US (552MPa < US < 793MPa) for an fatigue evaluation acc. ASME Section VIII Div 2.
In the 1989 Addition i found at page 564 "Where curves for various strength levels of a material are given, linear interpolation may be used for intermediate strength levels of these materials".
Unfortunately I can not find anything similar in the latest Versions (2007 - 2015)
Has someone experience with this issue?
Thank you in advance
Markus