We have received SA 106 Gr B material with its certificate. However, as manufacturer, we want to use the same material as SA 106 Gr C for an ASME Section I job, provided all specification requirements as per SA 106 Gr C are fulfilled, as demanded by PG 10. Is there a code interpretation that allows the same?
 
Replies continue below

Recommended for you

So what you are really asking for is dual certification specification. This can be done by the supplier, and not under PG-10. PG-10 really deals with unidentified material which could have been produced under a permitted specification, and material supplied under a specification not permitted by Section I.

Both SA 106 Grades are permitted under Section I and both are permitted.
 
C t.s. is higher than B. C can substitute B but not the other. Metenger, supplier cannot change specs, Am I wrong.
 
The pressure vessel manufacturer or the supplier of the material may re-certify it per PG-10 if the material meets all the requirements of the specification. See ASME Code interpretations 1-92-6 and 1-92-49.
 
@GenB
The tensile properties between Grades B and C allow for some overlap based on minimums, and a difference of only 10,000 psi. I think dual certification is possible.
 