rmillercwi
Materials
Asme sect 1 pressure vessel. Unit has been in service for several years.
Simple bracket made out of 1/4" thk CS plate welded directly to the O.D. of a 10" sch 120 1.25cr pipe. 3/8" fillet weld. 10" sch 120 pipe is .844 thk. (above 5/8")
ASME Sect 1 for P4 materials. I read this joint configuration to be exempt from PWHT provided a 250 f preheat is applied as long as the fillet weld is under 1/2".
The contractor is insistent on performing PWHT based on evaluation of current code verbiage based on the thickness of the basemetal beyond 5/8" thk. and thus the exemption is not applicable. In my opinion, PWHT is not required here.
Simple bracket made out of 1/4" thk CS plate welded directly to the O.D. of a 10" sch 120 1.25cr pipe. 3/8" fillet weld. 10" sch 120 pipe is .844 thk. (above 5/8")
ASME Sect 1 for P4 materials. I read this joint configuration to be exempt from PWHT provided a 250 f preheat is applied as long as the fillet weld is under 1/2".
The contractor is insistent on performing PWHT based on evaluation of current code verbiage based on the thickness of the basemetal beyond 5/8" thk. and thus the exemption is not applicable. In my opinion, PWHT is not required here.