Im trying to understand what rules must be followed to write a WPS containing more than one weld process from multiple single process PQRs. 200.4(a) paragraph 1 sentence 2 and paragraph 3 indicate that a WPS can have more than 1 welding process. Without looking at 200.4(b) yet, may this be done with multiple single process PQRs of any thickness?
For example can I use a 1/4" full pen. groove GTAW PQR and a 7/16" full pen. groove SMAW PQR (Same P#s) to write a WPS with a base metal range of 3/16" - 7/8", a 1/2" GTAW deposit t, a 7/8" SMAW deposit t, with all other essential variables per their respective process PQRs?
or can these single process PQRs not be combine into a multiple process WPS unless they meet the requirements of 200.4(b)? Also put, is a multiple process PQR the only way to get a multiple process WPS for PQR coupons less than 1/2"?
For example can I use a 1/4" full pen. groove GTAW PQR and a 7/16" full pen. groove SMAW PQR (Same P#s) to write a WPS with a base metal range of 3/16" - 7/8", a 1/2" GTAW deposit t, a 7/8" SMAW deposit t, with all other essential variables per their respective process PQRs?
or can these single process PQRs not be combine into a multiple process WPS unless they meet the requirements of 200.4(b)? Also put, is a multiple process PQR the only way to get a multiple process WPS for PQR coupons less than 1/2"?