May 7, 2003 #1 forgemaster Mechanical Joined May 7, 2003 Messages 5 Location GB Can anybody supply me with the chemical composition and mechanical properties for ASME SA- 350-LF2 or ASTM A-350.
Can anybody supply me with the chemical composition and mechanical properties for ASME SA- 350-LF2 or ASTM A-350.
May 7, 2003 1 #2 samuelliu Mechanical Joined Jan 7, 2001 Messages 85 Location CA Carbon, max 0.30; Manganese 0.60¨C1.35; Phosphorus,max 0.035; Sulfur, max 0.040; Silicon 0.15¨C0.30; Nickel 0.40 max; Chromium 0.30 max; Molybdenum 0.12 max; Copper 0.40 max; Columbium 0.02 max; Vanadium 0.05 max. Tensile strength, 70¨C95 ksi; Yield strength, min, 36 ksi. Upvote 0 Downvote
Carbon, max 0.30; Manganese 0.60¨C1.35; Phosphorus,max 0.035; Sulfur, max 0.040; Silicon 0.15¨C0.30; Nickel 0.40 max; Chromium 0.30 max; Molybdenum 0.12 max; Copper 0.40 max; Columbium 0.02 max; Vanadium 0.05 max. Tensile strength, 70¨C95 ksi; Yield strength, min, 36 ksi.