Hello Guys

According to ASME SA 333, Gr. 6 Product should be Quench and Tempered but we don’t have the facility. Any how we do achieve the properties required by the said standard through simple heat treatment furnace. In your opinion, does our product qualify according to the standard?

Regards

 
Replies continue below

Recommended for you

Send the piece out to a heat treatment facility under subcontract. You have the responsibility to ensure compliance with SA 333.
 
SA-333 Gr 6 does not mandate Q&T; per 4.2.1.5 it may be quenched & tempered. You need to review all of section 4.2.1 of the spec.

 