Hi,

I am trying to determine the allowable basic stress intensity (Sm) for stainless steel type 304. I have found the equivalent grade from ASME to RCCM which is Z6CN18.09, however, it is not referenced in the Z-Technical Appendices.

Has anyone else came across this problem?
Thanks
 
Replies continue below

Recommended for you

What product form? Plate, forging, welded pipe, seamless pipe, etc...
 
sorry missed this from original post - it is plate.
 
TGS4, do you have any guidance on this matter?
regards
 
Are you looking for the allowable stress in ASME (in which case, I would ask you which Section/Division), or RCC-M? And at what temperature? Are you looking for the straight grade of 304, the L grade, or the H grade?
 
Thanks for your reply. I am looking for the allowable stress in RCC-M. The temperature is 300 deg, in ASME it states 116MPA. However, in RCC-M the AFNOR GRADE is Z6CN18.09 which I cannot find in Table Z. It is the straight grade for 304 - I have the equivalent for 304L although I would rather reference the relevant grade.
many thanks
 