Hello all,
I am having a issue regarding the approval of ASME SA240-316L for PED using PMA(partial material appraisal).
As per the PMA, the values Re, Re,t, Rm, Rm,t shall be indicated.
Per PED 2014/68/EU, 7.1.1, Re for Austenitic steel is the 1.0% proof strength, and Re,t is the 1.0% proof strength at the design Temp.
Per PED 2014/68/EU, 7.1.2, The permissible general membrane stress, if the elongation after rapture exceeds 35% is the lesser of Re,t/1.2 and Rm,t/3 (Where Rm,t is the Tensile at the design Temp).
The NoBo(Notified Body) require to indicate the values of Re, Re,t, Rm, Rm,t and to satisfy the requirement of 7.1.2.
As far as I know, ASME II-D does not indicate the 1.0% values, and the Sy values of ASME II-D are the 0.2% values.
using the those values (from ASME II-D) will not satisfy 7.1.2.
Please advise.
I am having a issue regarding the approval of ASME SA240-316L for PED using PMA(partial material appraisal).
As per the PMA, the values Re, Re,t, Rm, Rm,t shall be indicated.
Per PED 2014/68/EU, 7.1.1, Re for Austenitic steel is the 1.0% proof strength, and Re,t is the 1.0% proof strength at the design Temp.
Per PED 2014/68/EU, 7.1.2, The permissible general membrane stress, if the elongation after rapture exceeds 35% is the lesser of Re,t/1.2 and Rm,t/3 (Where Rm,t is the Tensile at the design Temp).
The NoBo(Notified Body) require to indicate the values of Re, Re,t, Rm, Rm,t and to satisfy the requirement of 7.1.2.
As far as I know, ASME II-D does not indicate the 1.0% values, and the Sy values of ASME II-D are the 0.2% values.
using the those values (from ASME II-D) will not satisfy 7.1.2.
Please advise.