nnlpba
Materials
- Sep 19, 2005
- 6
I have a WPS that is qulaified for 0.120" to 0.480" that was welded with a root using GTAW Flux Cored Rod and filled out using solid GTAW rod. I have another WPS that was welded with GTAW Solid GTAW for the full thickness with a range of 0.074" to 0.864" (using 3 PQRs .148", .280" and .480"). Can I use the 2 WPS in a joint on 8" 0.594" wall.
The root would be performed using the Flux Cored TIG rood and the fill out woud be with GTAW solid rod? Or do I have to qualify another weld procedure using the Flux Cored TIG rod and GTAW fill out using at least a 0.300" wall material to cover the actual weld of 0.594"??
The root would be performed using the Flux Cored TIG rood and the fill out woud be with GTAW solid rod? Or do I have to qualify another weld procedure using the Flux Cored TIG rod and GTAW fill out using at least a 0.300" wall material to cover the actual weld of 0.594"??