Dear Members,

1)Can someone recommend any plate material that will be a closest ASME equivalent of “15NiCuMoNb5-6-4” DIN/EN plate material?
2)Does anybody have a general list of ASME equivalent plate materials for various DIN/EN plate materials? I would appreciate if it can be provided. That will be very helpful

Thank You & With Best Regards,
Parag Vora
 
Google : " equivalent ASME EN materials"
 
Dear RobyengIT,

On Internet it's mostly for Forgings, tubes and pipes.
There is no proper list for ASME equivalent for plates which am looking for.

Thanks for your response though.

Regards,
PV


 
Dear robyengIT,

Thank you very much for your time and helping me out with the EN-ASME equivalent materials. Thanks for guiding me and uploading the documents. I will review those and revert back in case of any additional questions.

Your assistance is very much appreciated.

With Regards,
Parag Vora
 