Jun 6, 2008 #1 cdi12 Structural Joined Jul 1, 2006 Messages 38 I am checking something I do not have ASME BTH-1 with me - are all allowable stresses Fy/3 even allowable bearing stress? Thanks, IV
I am checking something I do not have ASME BTH-1 with me - are all allowable stresses Fy/3 even allowable bearing stress? Thanks, IV
Jun 9, 2008 1 #2 RockEngineer Structural Joined May 29, 2002 Messages 267 Location US The allowable bearing stress between a pin and a plate per ASME BTH-1 eqn 3-51 is 1.25*Fy/Nd. Nd would normally be 3. If your pin rotates a large number of cycles they divide this by 2 for the allowable bearing per eqn 3-52. Upvote 0 Downvote