There was a change in the July, 1 2023 release regarding Miscellaneous Requirements. T-451 "Coarse Grain Materials" is attached, but has been described by our NDE provider as all customers will be required to buy all weld mock-ups for any new and existing weld approvals. This will either cost customers an extremely large amount in mock-ups or force them into CR or RT again.

Just curious what everyone else has heard/ran into regarding this change.

 