engr2GW
Petroleum
- Nov 7, 2010
- 308
Hello, The min thickness for PWHT to be required used to be 3/4 inches. I only have the 2012 version of the document. Has it increased? I saw a document where 0.98 inches was required as minimum, but there was no reference. Has it changed from 0.75 inches?
Thank you in advance
As much as possible, do it right the first time...
Thank you in advance
As much as possible, do it right the first time...