According to B31.3 Para. 345.2.3(c) for closure welds, this may be done as long as all components have been leak tested successfully, undergo in-process examination as per Para. 344.7, and pass either 100% RT or 100% UT examination. This becomes a problem when the final closure weld is a socket-weld. Has anyone been able to develope and qualify either a UT or RT procedure that will satisfy the requirements for closure welds when they're a socket weld configuration? We've submitted test pieces, consisting of 1" sch. 80 pipe into 3000# SW ell's, to a few NDE companies, with level 3's, asking if they can develope a procedure for either RT or UT and so far none have been able to do so. Anyone else have any better luck?