Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations LittleInch on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

ASME B31.3-Impact testing requirements

Status
Not open for further replies.

Thuhuongengineer

Mechanical
Joined
Apr 6, 2013
Messages
68
Location
US
Hi everybody,
Refer table 323.3.1 ASME B31.3, Number of test pieces for CVN test requirement that: "One piece, thickness T, for each range of (a) One piece from each lot of material in each material thickness from T/2 to T + 6 mm specification and grade including heat treat(1⁄4 in.)" It mean that when we qualify welding procedure range thickness aplly for WPS: T/2 to T+6, correct or not.

But refer QW-403.6 anf QW-451 ASME IX Max range thickness apply for WPS is 2T.

Summary, if CVN require Max range thickness 2T or T+6 ?
 
B31.3 trumps ASME IX except when T + 6mm is > 2T or T/2 is < the minimum thickness qualified per ASME IX (not very likely).
 
Stanweld has answered your question.
The fabrication code (B31.3) takes precedence over ASME IX so it is T + 6 mm,
Regards,
Shane
 