Hi all,

I've been trying to find the definition of what material should be used for Curve A,B,C, and D on Fig. 323.2.2A. I reviewed Appendix A and Table A-1 and can't find any note that tells me which curve to use for A106/A333, and 1.25/2.25 Cr pipe. Can someone point the way for me? I guess the set up for the notes for this curve is different than the notes for Section VIII.
 
Thank you SJones for pointing it out for me. I found what I needed.
 