jmec87
Mechanical
- Nov 5, 2013
- 225
Table 323.2.2 box B-3 has been revised in the 2020 Edition of B31.3. This appears to be a new requirement for charpy testing after simulated PWHT that would apply to unlisted materials, unless the “comparable” listed material option in box 7 is used. Previously, charpy testing after welding (and PWHT) was required on the PQR for unlisted materials (based on the previous references in Box B-3 to Note 2), but this revision now requires charpy testing on all production heats/lots after (simulated) PWHT for unlisted materials. There is no similar requirement for listed materials with a design minimum temperature at or warmer than the minimum temperature in Table A-1.
Question 1: Is the above understanding about the new charpy testing after (simulated) PWHT on all production heats/lots for unlisted material (unless the “comparable” listed material option in box 7 is used) correct?
Question 2: Are there any listed materials that would be considered to have “comparable” “composition, heat treatment, and product form” to common oilfield 4130 quench and tempered 75K minimum yield strength materials?
Question 1: Is the above understanding about the new charpy testing after (simulated) PWHT on all production heats/lots for unlisted material (unless the “comparable” listed material option in box 7 is used) correct?
Question 2: Are there any listed materials that would be considered to have “comparable” “composition, heat treatment, and product form” to common oilfield 4130 quench and tempered 75K minimum yield strength materials?