I AM FULL PENETRATION WELDING 1/2" THK P1 MATERIAL TO P5A MATERIAL AND USING A BACKING BAR. CODE IS ASME B31.1. BOTH BASE MATERIALS HAVE CARBON < 0.15% TO AVOID POST WELD HEAT TREATMENT. BACKING BAR WILL P1 MATERIAL

QUESTION: IS IT A CODE REQUIREMENT THAT THE P1 BACKING BAR MATERIAL ALSO HAVE CARBON < 0.15%
 
Replies continue below

Recommended for you

Backing strip is a poor option for butt welding, try to avoid it.
ASME B31.1 (2018) 127.2.2 is clear.
Regards
 
Even though backing ring is not desirable, if you want to use it then base metal and backing ring metal shall be compatible as per Cl. 127.2.2. So C content should be less than 0.15 %. Also regarding PWHT please check Table 132.2-1 for Mandatory requirements and exemptions. The backing ring should be removed after welding as indicated in ASME B31.1.