DM2
Mechanical
- Oct 20, 2007
- 147
In looking at the SE values for ASTM A-53, Grade A Seamless pipe it appears that the safety factor changes between the 2001 and 2007 edition. In both editions the Tensile strength and Yields are the same but the SE value, as 650°F in the 2007 edition is 13.7 ksi, and in 2001 it's 12.
The 2007 edition seems to use a safety factor of 3.5, where as the 2001 edition seems to use a safety factor of 4.0.
Am I reading this right?
Why the change from 2001 to 2007?
Regards,
Dan Marr
"Real world Knowledge isn't dropped from a parachute in the sky but rather acquired in tiny increments from a variety of sources including panic and curiosity."
The 2007 edition seems to use a safety factor of 3.5, where as the 2001 edition seems to use a safety factor of 4.0.
Am I reading this right?
Why the change from 2001 to 2007?
Regards,
Dan Marr
"Real world Knowledge isn't dropped from a parachute in the sky but rather acquired in tiny increments from a variety of sources including panic and curiosity."