A certain fabricated skid used an SS flange connection for an instrument connection. The SS flange has a lower max allowable pressure than the rest of the CS class 150 flange rating. The design pressure of the system is marginally over the SS flange rating by a fraction of a bar. Is there any provision in the code that may exempt the use of the SS flange at the marginal excess over the flange rating.