I'm doing a vessel test plate that is 4.7" thick and has to be tested to PW 53.9. Everything is pretty standard with exception to the bend test.
53.9.1 says the width of the transverse bend specimen is to be 1.5 "T" which makes the specimen width 7".
Is this the true intent?
53.9.1 says the width of the transverse bend specimen is to be 1.5 "T" which makes the specimen width 7".