Hi,
Recently i have noticed that the ASME VIII Div.1 vessels we manufacture use AS3678 plate for non pressure parts (in lieu of SA-36). We also use AS1548 but of course this an accepted material in II Part D.
I cant find any reference to AS3678 in part II D , but was wondering if there is a paragraph somewhere in div 1 that allows the use of this material for structural supports / trays etc.
I seem to recall a paragraph somewhere talking about other steels may be substituted as long as they are of weldable quality and met certain composition requirement.
Regards,
Richard
Recently i have noticed that the ASME VIII Div.1 vessels we manufacture use AS3678 plate for non pressure parts (in lieu of SA-36). We also use AS1548 but of course this an accepted material in II Part D.
I cant find any reference to AS3678 in part II D , but was wondering if there is a paragraph somewhere in div 1 that allows the use of this material for structural supports / trays etc.
I seem to recall a paragraph somewhere talking about other steels may be substituted as long as they are of weldable quality and met certain composition requirement.