Hi all,
I'd like to know how elastic modulus for 32MPa of various curing day concretes can be determined
e.g. 7days/ 14 days/ 28 days/ 30yrs
Is it okay to assume that because creep and shrinkage effects are so miniscule in 7 , 14 and 28 day concretes,
modulus of elasticity are taken as:
(rho^1.5) x (0.043x SQRT(fcmi)) for fcmi <40MPa
(rho^1.5) x (0.024x SQRT(fcmi)+0.12) for fcmi > 40MPa
Whilst for 30yr concretes, since creep and shrinkage must be accounted for, one must use coefficient of shrinkage to find
Ec.
Plus,could anyone englighten me on matters associated with the behaviour of 7day,14day and 30yr concrete cylinder before/after they're cracked and how the the choice of concrete may influence the calculations of Ix or Ec and etc etc. Anything relevant would be good.
cheers
I'd like to know how elastic modulus for 32MPa of various curing day concretes can be determined
e.g. 7days/ 14 days/ 28 days/ 30yrs
Is it okay to assume that because creep and shrinkage effects are so miniscule in 7 , 14 and 28 day concretes,
modulus of elasticity are taken as:
(rho^1.5) x (0.043x SQRT(fcmi)) for fcmi <40MPa
(rho^1.5) x (0.024x SQRT(fcmi)+0.12) for fcmi > 40MPa
Whilst for 30yr concretes, since creep and shrinkage must be accounted for, one must use coefficient of shrinkage to find
Ec.
Plus,could anyone englighten me on matters associated with the behaviour of 7day,14day and 30yr concrete cylinder before/after they're cracked and how the the choice of concrete may influence the calculations of Ix or Ec and etc etc. Anything relevant would be good.
cheers