I understand that welding of reinforcing is to be avoided but looking through AS1554 there doesn’t seem to be anything overly prohibitive there?
Am I correct in saying that if class N reinforcing is welded in accordance with Table 3.2 (ie W50X) no reduction in strength is required? Or are some intensive testing proceedures required?
I have only used welded reinforcing for cast-in-plates, tags etc..and adopted a 250 MPa yield stress for class N reo that has been hit with a weld, due to inhouse direction. Is this too conservative?
Thanks!
Am I correct in saying that if class N reinforcing is welded in accordance with Table 3.2 (ie W50X) no reduction in strength is required? Or are some intensive testing proceedures required?
I have only used welded reinforcing for cast-in-plates, tags etc..and adopted a 250 MPa yield stress for class N reo that has been hit with a weld, due to inhouse direction. Is this too conservative?
Thanks!