AS PER UCS-56 DOES PWHT ASSESSED BASED ON WELD THICKNESS OR VESSEL THICKNESS

Status
Not open for further replies.

staticmh

Mechanical
Joined
Aug 28, 2019
Messages
57
Location
AE
Hi Folks!

This has been an quite significant misconception in regard of ASME Sec VIII Div. 1 UCS-56 PWHT criteria.

Please any body correct me that PWHT is always being assessed based on the maximum weld thickness or it can also be done based on vessel metal thickness.

I'm designing a vessel and it contain a top body blind flange of having thickness of 150mm (With Raised face) & 148mm (Without 2mm Raised face)

There is a one NPS-4" nozzle welding with RF Pad as set on, instead of set in. The reason that Why i'm using set on is that, as per my understanding i am exempting the PWHT not to calculate the higher weld thickness (Above 38mm) which can conclude the PWHT as per UCS-56 and saving the cost of PWHT.

Below is my case all the welds shown as per exact situation.

NPS-4_INCH_knnhlq.jpg


148mm is the Blind flange thickness.


Please advice whether PWHT shall be yes for this case or NO ?
 
@ staticmh
Do you consider this PV for low temperature service? Why?

Regards
 
The more I read the more confused I become.
The Code can make for awkward reading, but the information is all in there - know your definitions.

"Everyone is entitled to their own opinions, but they are not entitled to their own facts."
 
@ staticmh

As you said on 7Mar21 MDMT = 0º C, then this PV is not “Low Temperature Operation” UCS-65 and impact test is not required.

Regards
 