Eng-Tips is the largest forum for Engineering Professionals on the Internet.

Members share and learn making Eng-Tips Forums the best source of engineering information on the Internet!

  • Congratulations JStephen on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Arc Spray to Face of Thrust Collar Base Metal : SS304

BioMechanic001

Mechanical
Joined
Mar 23, 2021
Messages
1
Location
GB
We need to repair face of Thrust Disc with details below.
Thrust Dis Material : SS 304

OD of Disc: 275 mm
Thickness of flange : 28.50 mm
Coating Thickness : 1 mm
Service provider suggested to use SS420 wire. Now we need to verify the compatibility of coating material with base material SS304 based on the standard ASME Section II.

  • Is this SS420 Wire is compatible with the base material SS304?
  • Based on the standard ASME Section II is it acceptable to use the SS420 wire for the coating on SS304 Material?
 

Attachments

  • Location at Face to be Repaired.jpeg
    Location at Face to be Repaired.jpeg
    191.2 KB · Views: 3
What is the purpose of the overlay?
This isn't a code issue it is an application issue.
If this isn't a pressure boundary the Code doesn't care.
What was on it before?
Did it work?
I hope that the loads are very low.
304 is soft and makes a poor substrate.
 