hi
we bought used arc furnace.we need 2 or 3 pieces of 15 cm dia graphite electrode for test furnace.but electrode suppliers dont sell retail electrode.we must buy min 20 ton electrode.but they are very expensive.does anyone know is there any way for made 15 cm dia graphite electrode in our workshop?we need only 2 or 3 pieces electrode.
thanks
 
Replies continue below

Recommended for you

Dear arash2545,

Visit nearby steel industries where they have arc furnace and try for 2/3 electrodes.