Is ASTM E140 Table 3 (high nickel alloy) the appropriate table for converting microhardness to Rockwell for 304L stainless steel?
 
Replies continue below

Recommended for you

Are you dealing with annealed material?
Or has it been worked to some higher hardness?
And what scales are you trying to convert between?

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 
Either cold worked or annealed. I need to be able to convert between microhardness (Knoop/Vickers) and Rockwell.
 
For the cold worked material you will need to build your own conversions.
I have never found the tables to be great for that, but you could use the Ni alloy table in a pinch.
I had better luck converting from Superficial Rockwell scales.
For annealed material it is tougher because you usually can't use Superficial Rockwell.
Isn't there a table marked Austenitic Steels? That might be closer for annealed products.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 
Concur with EdS.
I will not accept conversion (ASTM E140) from microhardness to macrohardness. If I must do it I will use a reference block of similar composition in a similar condition.

"Everyone is entitled to their own opinions, but they are not entitled to their own facts."
 