Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations JStephen on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Applicable of WPS

Status
Not open for further replies.

duongwe

Mechanical
Joined
Jan 25, 2011
Messages
43
Location
VN
Dear all,

i had a approved WPS (ASME IX) with contents as below:

Consumable ER 70S-6/E 7018
Process: GTAW/SMAW
Material: P No.1 Gr.1 to P No.1 Gr.1
Diameter: 75 and Over
Thickness: 4.8 to 19.0 mm
Position: 6G

can i weld this WPS for 75 and Over diameter with GTAW only???

Please explain for me.
 
Maybe.

Refer to QW-200.4(a)(1) which says that you can use one process (i.e. GTAW) from a WPS which was performed with more than one welding processes (i.e. GTAW/SMAW), providing the required variables are applied and (2)deposits welded and base metal thickness meet QW-451.

I believe (2) will be your constraint. If the deposited weld was enough to cover the maximum qualified limit of your proposed joint then you should be good to go.

 
hi all...

excuse me..
i want to ask about pipe diameter range.
where i should refer to know how the diameter range to use.

regard.

 
yazid89,
You don't - diameter qualified should not be listed on a WPS,
Regards,
Kiwi
 
yazid89,
Diameter range qualified is in Welder Performance qualification - not in WPS qualification. You appear to be confusing the requirements of API 1104 with the requirements of ASME IX.

 
Just make an "administrative" revision to that WPS to give it a Diameter Range of "ALL".

As stanweld said, it is not an Essential or Supplementary Essential Variable for a WPS. Get rid of that ridiculous limitation with a revision to the WPS. Until that limitation is gone, you cannot 'legally' weld anything over 20.
 