This question pertains to seal welding of tube-to-tubesheet joints per ASME Sec. VIII, Div. 1.
Does anyone know if App. A is required for seal welded tubes, since they are not covered by UW-20?
In my particular case, I have 2205 Duplex Tubes seal welded to SA-516-70N Tubesheets (Fixed TS exchanger). The problem I am having is that if I follow App. A, A-2 for definition of Fy, it states that qualification testing is required when tubesheet-to-tube yield stress ratio falls below 0.6. In my case at the specified operating temp's, Fy=0.44. We will not be performing any qualification testing, so this violates App. A requirements.
I know app. A is listed as non-mandatory, but our latest design software continues to tack app. A onto the end of the UHX tubesheet calcs.
I just want to be sure there is no reference in the code that invokes App. A for seal welding so that I can ignore the Fy ratio requirement.
Any help on this is greatly appreciated.
Does anyone know if App. A is required for seal welded tubes, since they are not covered by UW-20?
In my particular case, I have 2205 Duplex Tubes seal welded to SA-516-70N Tubesheets (Fixed TS exchanger). The problem I am having is that if I follow App. A, A-2 for definition of Fy, it states that qualification testing is required when tubesheet-to-tube yield stress ratio falls below 0.6. In my case at the specified operating temp's, Fy=0.44. We will not be performing any qualification testing, so this violates App. A requirements.
I know app. A is listed as non-mandatory, but our latest design software continues to tack app. A onto the end of the UHX tubesheet calcs.
I just want to be sure there is no reference in the code that invokes App. A for seal welding so that I can ignore the Fy ratio requirement.
Any help on this is greatly appreciated.