I am buying API 5L X65 PSL2 plates 39mm thk. We asked for normalized plates but the mill says that this cannot be possible becouse the plates sour resistance will be lost with the normalizing temperature (about 600°C).
They propose TMCP plates without possibility of PWHT.
I need the plates for welded pipes according B31.3 and I need to perform two PWHT's at 593-605°C (one during the pipe fabrication and one during the site erection.
How do you think I have to procede?
Thank you for your co-operation