Aug 24, 2019 #1 JXWu Petroleum Joined Oct 26, 2015 Messages 24 Location TH Dear experts, Is it a API 650 requirement that the second side of a double-side welded joint needs to be back-chipped at least one-third of the joint thickness? I cannot find this requirement in the API 650 12th edition. Need advice. Thanks
Dear experts, Is it a API 650 requirement that the second side of a double-side welded joint needs to be back-chipped at least one-third of the joint thickness? I cannot find this requirement in the API 650 12th edition. Need advice. Thanks
Aug 26, 2019 #2 Dhurjati Sen Materials Joined Dec 14, 2017 Messages 1,001 Location IN Dear JXWu, Are you constructing a double-walled dome roofed tank? Regards. DHURJATI SEN Kolkata, India Upvote 0 Downvote
Dear JXWu, Are you constructing a double-walled dome roofed tank? Regards. DHURJATI SEN Kolkata, India
Aug 26, 2019 Thread starter #3 JXWu Petroleum Joined Oct 26, 2015 Messages 24 Location TH This is a API 650 single wall cone roof tank Upvote 0 Downvote