Aug 13, 2020 #1 Scary999 Industrial Joined Aug 13, 2020 Messages 3 Location US What is the maximum that a lap welded top angle can extend past the top of the shell plate?
Aug 14, 2020 #2 LittleInch Petroleum Joined Mar 27, 2013 Messages 22,973 Location GB Try posting this in the storage tank forum perhaps?? Remember - More details = better answers Also: If you get a response it's polite to respond to it. Upvote 0 Downvote
Try posting this in the storage tank forum perhaps?? Remember - More details = better answers Also: If you get a response it's polite to respond to it.
Aug 16, 2020 #3 IFRs Petroleum Joined Nov 22, 2002 Messages 4,680 Location US According to API 650 figure F.2, twice the shell plate thickness is the max the heel of the angle can extend above the tank shell. Upvote 0 Downvote
According to API 650 figure F.2, twice the shell plate thickness is the max the heel of the angle can extend above the tank shell.
Aug 20, 2020 #4 LAZAR90 Petroleum Joined Aug 17, 2020 Messages 24 Location MU I believe this will help you. https://files.engineering.com/getfile.aspx?folder=74f675c4-88cd-4652-9b48-445479308a40&file=TOP_ANGLE.pdf Upvote 0 Downvote