sollapalooza
Mechanical
Hello
I would like to ask about storage tank fabrication sequence, I do not find anything regarding to this in API 650. A fabricator plans to do blasting + primer on all plates prior to rolling, then transport them plates to site and finish all the welding + final coat. Is this a good practice?
Personally I foresee a lot of touch up needs to be done at site since the primer may be damaged by the rolling machine. On top of that, the surface profile generated from blasting may be ruined by the rolling machine as well.
Should we proceed with the sequence (blast+prime -> roll -> final coat), is there any code that specifies acceptance criteria of the surface profile and primer? I think not all damaged profile has to be repaired.
I would like to ask about storage tank fabrication sequence, I do not find anything regarding to this in API 650. A fabricator plans to do blasting + primer on all plates prior to rolling, then transport them plates to site and finish all the welding + final coat. Is this a good practice?
Personally I foresee a lot of touch up needs to be done at site since the primer may be damaged by the rolling machine. On top of that, the surface profile generated from blasting may be ruined by the rolling machine as well.
Should we proceed with the sequence (blast+prime -> roll -> final coat), is there any code that specifies acceptance criteria of the surface profile and primer? I think not all damaged profile has to be repaired.