Dear All,
In API 650 Ed. 12th 2016, it states that The tank is self-anchored providing the following conditions are met:
(4) The required annulus plate thickness does not exceed the thickness of the bottom shell course.
Based on the above statement, if the tank is self-anchored, the thickness of bottom annular plate can not exceed the thickness of first shell of the tank. Am I translating this, right?
If I am right, I would be confused then, because I have seen an API tank with annular bottom thickness is greater than the thickness of first shell of the tank.
Please help me with this section of API.
Thanks!
In API 650 Ed. 12th 2016, it states that The tank is self-anchored providing the following conditions are met:
(4) The required annulus plate thickness does not exceed the thickness of the bottom shell course.
Based on the above statement, if the tank is self-anchored, the thickness of bottom annular plate can not exceed the thickness of first shell of the tank. Am I translating this, right?
If I am right, I would be confused then, because I have seen an API tank with annular bottom thickness is greater than the thickness of first shell of the tank.
Please help me with this section of API.
Thanks!