I've been looking at API 650 table 3-6 for regular style re-pad nozzle elevations. Table 3-6 column 8 footnote d says that the HN dimensions are for Appendix A tanks only. Looking at Appendix A, section A.5.2, all you need to watch out for is 2 1/2 times the shell thickness between toes of welds. These yield different minimum nozzle elevations. For example, for a 4" nozzle, table 3-6 says 9" is the lowest a regualr type nozzle can be but if you calculate per section A.5.2 for a 1/2" shell and 1/2" bottom the number is 6 + .5 + .5 + 2.5 * .5 = 8 1/4". This number gets lower for thinner shells and bottoms. Am I possibly misinterpreting A.5.2? If I am reading A.5.2 correctly, why does table 3-6 have footnote d written as it is?