Hi,
I had a doubt on my QC department that created a procedure of air leak test with below requirement:
Pressure: 1 bar
Holding time: 5 min
Additional: Soap solution
Can anybody here help me to clarify this requirement, Besides that I can't find any requirement on the 1 bar pressure with holding time of 5min in API 650.
Thank
Marvin
I had a doubt on my QC department that created a procedure of air leak test with below requirement:
Pressure: 1 bar
Holding time: 5 min
Additional: Soap solution
Can anybody here help me to clarify this requirement, Besides that I can't find any requirement on the 1 bar pressure with holding time of 5min in API 650.
Thank
Marvin