Water Injection pipeline about 8 km
Design Pressure 139 Bar, above ground.
Solar radiation temp 95 c.degree, design temp 75 c.degree.
Peoject Spec for Line pipe, APL 5L X52 PSL 2, WT 17.5mm. 3PE coating.
However, only APL 5L X52 PSL 1 is market available. Could PSL 1 be alternative to PLS 2 technically?
Thanks for any tips.
David
Design Pressure 139 Bar, above ground.
Solar radiation temp 95 c.degree, design temp 75 c.degree.
Peoject Spec for Line pipe, APL 5L X52 PSL 2, WT 17.5mm. 3PE coating.
However, only APL 5L X52 PSL 1 is market available. Could PSL 1 be alternative to PLS 2 technically?
Thanks for any tips.
David