Experts,

Can anyone tell me what the difference is between API 5L Gr.X42 and API 5L Gr.X42R?

Is there a difference?

Our project specs out API 5L PSL-2 Gr.X42 - this is what we ordered. What we received is marked Gr.X42R - the MTR also refers to Gr.X42R.

I'm looking in API Spec. 5L and can't seem to find anything about Gr.X42R.

numberfive
 
Replies continue below

Recommended for you

Look at table 3.

R means "as rolled" without any further mechanical or heat treatment

My motto: Learn something new every day