Refer to NACE MR0175-2003 Table D-2, material API 5L Grade A & B, Grade X-42 through X-65 have been accepted for sour service
But I don't find the limitation value of H2S partial pressure in both of API Spec 5L and NACE MR0175.

Can anyone explain this limitation?
 



for gasoil services, above .01 Mol % of H2S and at temperatures above 396ºC you begin to have higher and higher corrosion rates for the carbon steels