Hi all,
We have been asked by a client to use existing API 5CT tubing (5", L80 GRE lined, threaded ends) as pipeline material for a water injection network.
I can't see anything in ASME B31.4 stopping us from using this material, but we are a bit stuck on how to handle branches off the main line, and connections to valves, instruments etc which will be standard 6" items.
We are trying to do the system to standards and stress the complete system (Caesar II)
Has anybody done the above, or can they recommend how to handle the fittings and transitions to standard pipe sizes?
Regards
Stephen
We have been asked by a client to use existing API 5CT tubing (5", L80 GRE lined, threaded ends) as pipeline material for a water injection network.
I can't see anything in ASME B31.4 stopping us from using this material, but we are a bit stuck on how to handle branches off the main line, and connections to valves, instruments etc which will be standard 6" items.
We are trying to do the system to standards and stress the complete system (Caesar II)
Has anybody done the above, or can they recommend how to handle the fittings and transitions to standard pipe sizes?
Regards
Stephen