Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

API 570 Para. 8.2.8(d) - Grammar Interpretation

Status
Not open for further replies.

marty007

Mechanical
Joined
Mar 8, 2012
Messages
622
Location
CA
Hey everyone,

Grammar question here for interpreting codes...

API-570 paragraph 8.2.8(d) - associated with closure welds:
d) MT or PT shall be performed on the root pass and the completed weld for butt welds and on the completed weld for fillet welds.

Question: for socket weld closure welds, allowed per para 8.2.8(b)(2), do I need to perform MT or PT on the root pass?

Thank you,
Marty
 
No, but you should left a gap of 1 or 1,5 mm for dilatation

Regards
 
No root pass in fillet weld.
MT or PT in the finished fillet weld.

Regards
 