I have following scenario for a safety valve.
MAWP = 240bar g, set pressure = 240 bar g, operating temperature = 50 deg c, relieving temperature = 580 deg c., over pressure = 21% and valve body material is carbon steel. Vendor has calculated and selected 1.5D3 valve with 2500# x 300# rating. Vendor says that 2500# rating is selected based on API 526. Can anybody explain me how to cross check this with API 526 table 3? Why I can not select 1500# valve? Thanks in advance.
MAWP = 240bar g, set pressure = 240 bar g, operating temperature = 50 deg c, relieving temperature = 580 deg c., over pressure = 21% and valve body material is carbon steel. Vendor has calculated and selected 1.5D3 valve with 2500# x 300# rating. Vendor says that 2500# rating is selected based on API 526. Can anybody explain me how to cross check this with API 526 table 3? Why I can not select 1500# valve? Thanks in advance.