Can anyone please help me out with a cut condition for clean cutting 11 ga stainless steel with nitrogen on a 1500 watt mazak stx 48?


Thank
 
These are for a 1300 watt. For a 1500 watt just change the P1300 to P1500.

%
O8120
(SSN2 120)
(LENS 7.5)
(NOZZLE 2.0MM)
(FOCUS -0.100)
(PECK PIERCE)
G88P10M58
G87P20
G82P1300Q500R100
M32
M20
M22
G04X0.5
M99
%

%
O8121
//(SSN2 120)
//(FAST)
//(FEEDRATE 57)
G82P1300Q500R100F57.0
M54 (11.0KG)
G87P-3
G181R25
G04X0.5
M99
%

%
O8122
//(SSN2 120)
//(MEDIUM)
//(FEEDRATE 45)
G82P850Q500R100F45.0
M54 (11.0KG)
G87P-3
G181R25
G04X0.5
M99
%

%
O8123
//(SSN2 120)
//(SLOW)
//(FEEDRATE 20)
G82P1300Q500R50F20.0
M54 (11.0KG)
G87P-3
G04X0.5
M99
%

%
O8126
//(SSN2 120)
//(LEADIN)
//(FEEDRATE 12)
G82P1300Q500R100F12.0
G88P50M58