Hi,

we have the laser in the subject line, the techs that help set it are telling us we HAVE to run nitrogen, but everyone else, even sales is telling us No.

we are cutting mild gauge steel and galv for the most part. how do we get settings or set up to run facility air?
'
thanks for any help
 