I have come across a bell & spigot joint pulling out in front of a thrust block. Except for a small concrete plinth supporting the dead weight of the pipe body the joint has not been restrained and is part of an above-ground installation to a 62" welded pipe system. The below ground portion is bell & spigot throughout after the thrust block.
Can anybody point out if such practice, of having above ground unrestrained bell & spigot joint, is widespread? or if there code or good engineering practice that disencourage such installation? Some previous examples if exist would be appreciated.