We are designing a bridge and the client has requested that all vertical concrete surfaces be coated to prevent graffiti. We have not specified this before, but from looking on the internet, I see there are sacrificial and permanent coatings available.

Anyone have any experience with either? Recommendations on which type is better?

Thanks
 
Replies continue below

Recommended for you

One solution is,that you contact a few supliers of anti graffiti coating. Than you have 'll have a clear what is usefull for your applience. and what is on the market.



Signature: I'm dutch and I'll do my best on my English;)
 
I was marginally involved on the selection of an antigraffiti coating on a previous job, in fact some elements were 'marked' before constructio finished. We could not find anything really effective. All treatments were really temporary and involved regular re-application and strong power washing and scrubbing to remove the graffiti anyway.

Finaly we opted for not doing anything and paint over the graffiti with a concrete colour paint immediately after it would be discovered. Apparently the artist loose interest if after spending a considerable amount of time the 'art' is covered next morning without anybody seeing it.

I would be interested if you find anything effective though. I could use it on future jobs
 
Ever hear about how the media boosted the proliferation of grafitti in NYC?

A TV newscaster once highlighted grafitti, and the grafitti kids responded in droves hoping to be featured on TV.

I would like to hear about how NYC finally brought this to a screeching halt. Jail time and bills to the parents probably helped.
 
Here's TxDOT's list of approved anti-graffiti coatings:

ftp://ftp.dot.state.tx.us/pub/txdot-info/cmd/mpl/antigraf.pdf

They've been pleased with the "permanent, water-cleanable" type at the bottom. Those are the ones where the graffiti paint doesn't really adhere. (Disregard the highlighting; that just shows a change from the previous version.)