Anyone have any experience with the use of nelson stud welding to attach antenna mounts to elevated water storage tanks? The structural part is OK, but I'm trying to determine the extent of damage, if any, to expect on the interior coating of the tank. The proposed studs are 3/8" dia and the tank plate is 1/4" thick. Nelson says everything is fine and don't worry, but they'll be gone in a year and I'll still have a tank to maintain. Anybody have any problems with interior coating burn when a antenna was put on your tank?