Hello all
Any tips hints directions to solving my problem are much appreciated!
I am trying to model a composite sandwich structure using a orthotropic core material that has a non-linear deformation curve. I am using TB,PLASTIC,,,,MISO and so far I am getting results, however I don't trust my results. The non-linear table I input gets surpassed by quite a bit. It is defined up to a strain of 7.32%, for which the stress is 1.57MPa and at which the stiffness slope is 0. I would have expected Ansys to stick to this defined material data, however it's computed stresses and strains for elements with these material properties are up to 70$ and 6MPa stress.
I don't quite know where to look for a solution to this. The fact that strains go outside of the defined region seems normal since the final stiffness is zero. However I feel they should still remain at their maximum defined stress. I will try to use TB,MISO however I am pretty sure this will not have a significant effect on the results. If this doesn't work, I think I will try to 'kill' the elements once they reach a certain stress/strain value, however I was hoping there was an easier way to obtain a realistic stress-strain distribution in my model.
Thanks a lot for your time!
I have defined my plastic material in the following way;
et,2,solid185
MP,EX,2,45
MP,EY,2,45
MP,EZ,2,45
MP,GXY,2,22
MP,GYZ,2,22
MP,GXZ,2,22
MP,PRXY,2,0.42
MP,PRYZ,2,0.42
MP,PRXZ,2,0.42
TB,PLASTIC,2,1,26,MISO
TBTEMP,0
TBPT,DEFI, 0.000000000000000 , 1.003048937000000
TBPT,DEFI, 0.00162033300000000 , 1.073777736000000
TBPT,DEFI, 0.00360120700000000 , 1.125693844000000
TBPT,DEFI, 0.00504243800000000 , 1.156856602000000
TBPT,DEFI, 0.00684421000000000 , 1.193219388000000
TBPT,DEFI, 0.00900699100000000 , 1.229600879000000
TBPT,DEFI, 0.01116977300000000 , 1.265982370000000
TBPT,DEFI, 0.01423461000000000 , 1.307591947000000
TBPT,DEFI, 0.01693937200000000 , 1.338820173000000
TBPT,DEFI, 0.01910355700000000 , 1.359657696000000
TBPT,DEFI, 0.02126774100000000 , 1.380495218000000
TBPT,DEFI, 0.02487549400000000 , 1.406588884000000
TBPT,DEFI, 0.02776169700000000 , 1.427463817000000
TBPT,DEFI, 0.03136991800000000 , 1.448376160000000
TBPT,DEFI, 0.03353503700000000 , 1.458851037000000
TBPT,DEFI, 0.03624167100000000 , 1.469353971000000
TBPT,DEFI, 0.03894830400000000 , 1.479856906000000
TBPT,DEFI, 0.04237648800000000 , 1.495578573000000
TBPT,DEFI, 0.04724870900000000 , 1.511375061000000
TBPT,DEFI, 0.05103836900000000 , 1.521934111000000
TBPT,DEFI, 0.05518903900000000 , 1.532511866000000
TBPT,DEFI, 0.06078327800000000 , 1.548345764000000
TBPT,DEFI, 0.06565596600000000 , 1.558960930000000
TBPT,DEFI, 0.07034861700000000 , 1.564385419000000
TBPT,DEFI, 0.07323622300000000 , 1.569716383000000
TBPT,DEFI, 0.0735 , 1.569716383000000
Any tips hints directions to solving my problem are much appreciated!
I am trying to model a composite sandwich structure using a orthotropic core material that has a non-linear deformation curve. I am using TB,PLASTIC,,,,MISO and so far I am getting results, however I don't trust my results. The non-linear table I input gets surpassed by quite a bit. It is defined up to a strain of 7.32%, for which the stress is 1.57MPa and at which the stiffness slope is 0. I would have expected Ansys to stick to this defined material data, however it's computed stresses and strains for elements with these material properties are up to 70$ and 6MPa stress.
I don't quite know where to look for a solution to this. The fact that strains go outside of the defined region seems normal since the final stiffness is zero. However I feel they should still remain at their maximum defined stress. I will try to use TB,MISO however I am pretty sure this will not have a significant effect on the results. If this doesn't work, I think I will try to 'kill' the elements once they reach a certain stress/strain value, however I was hoping there was an easier way to obtain a realistic stress-strain distribution in my model.
Thanks a lot for your time!
I have defined my plastic material in the following way;
et,2,solid185
MP,EX,2,45
MP,EY,2,45
MP,EZ,2,45
MP,GXY,2,22
MP,GYZ,2,22
MP,GXZ,2,22
MP,PRXY,2,0.42
MP,PRYZ,2,0.42
MP,PRXZ,2,0.42
TB,PLASTIC,2,1,26,MISO
TBTEMP,0
TBPT,DEFI, 0.000000000000000 , 1.003048937000000
TBPT,DEFI, 0.00162033300000000 , 1.073777736000000
TBPT,DEFI, 0.00360120700000000 , 1.125693844000000
TBPT,DEFI, 0.00504243800000000 , 1.156856602000000
TBPT,DEFI, 0.00684421000000000 , 1.193219388000000
TBPT,DEFI, 0.00900699100000000 , 1.229600879000000
TBPT,DEFI, 0.01116977300000000 , 1.265982370000000
TBPT,DEFI, 0.01423461000000000 , 1.307591947000000
TBPT,DEFI, 0.01693937200000000 , 1.338820173000000
TBPT,DEFI, 0.01910355700000000 , 1.359657696000000
TBPT,DEFI, 0.02126774100000000 , 1.380495218000000
TBPT,DEFI, 0.02487549400000000 , 1.406588884000000
TBPT,DEFI, 0.02776169700000000 , 1.427463817000000
TBPT,DEFI, 0.03136991800000000 , 1.448376160000000
TBPT,DEFI, 0.03353503700000000 , 1.458851037000000
TBPT,DEFI, 0.03624167100000000 , 1.469353971000000
TBPT,DEFI, 0.03894830400000000 , 1.479856906000000
TBPT,DEFI, 0.04237648800000000 , 1.495578573000000
TBPT,DEFI, 0.04724870900000000 , 1.511375061000000
TBPT,DEFI, 0.05103836900000000 , 1.521934111000000
TBPT,DEFI, 0.05518903900000000 , 1.532511866000000
TBPT,DEFI, 0.06078327800000000 , 1.548345764000000
TBPT,DEFI, 0.06565596600000000 , 1.558960930000000
TBPT,DEFI, 0.07034861700000000 , 1.564385419000000
TBPT,DEFI, 0.07323622300000000 , 1.569716383000000
TBPT,DEFI, 0.0735 , 1.569716383000000